Layer Property | Results | Typical Value | Test Method |
Exterior Layer Performance Properties |  |  |  |
Dimension Stability
Flex Crack Resistance
Ink Recommendation
Stiffness / Flexibility
Tear Propogation
Tear Resistance (grams-force)
Chemical Resistance
Light
Moisture Vapor Trans Rate
Odor
Oxygen Vapor Trans Rate | Excellent
Good
Film Inks
Average
1700
700 MD / 700 CD
Excellent
Average
0.093
Average
45.9 | N/A
N/A
N/A
N/A
grams
grams-force
N/A
N/A
grams/100 sq. in./day
N/A
cc/100 sq.in./day | N/A
N/A
N/A
N/A
N/A
N/A
N/A
N/A
N/A
N/A
N/A |
Sealant Layer Performance Properties |  |  |  |
Caulk & Flow
Hot Tack
Puncture Resistance
Seal Initiation Temperature
Seal Strength
Seal through Contamination | Excellent
Excellent
21
240
3000
Excellent | N/A
N/A
Pounds of force
°F
g/in. @ 350°F/40 psi/0.5 secs
N/A | N/A
N/A
N/A
N/A
N/A
N/A |