Print this Page

Fasson® Laser CodeTM Drum Label TC/S4600/96#MF
Spec# 77742 - Obsolete
Facestock:
Fasson® 4 Mil White Flexible Topcoated Vinyl has good tear strength and weather resistance, but relatively low heat resistance. The 7050 topcoat enhances solvent and some water-based flexographic printing. This facestock is not recommended for UV printing. Please note that due to its highly filled topcoating, this facestock is not recommended for applications requiring the use of an overlaminate. Use of an overlaminate will cause a separation of the overlaminate from the facestock if the overlaminate is tampered with.



Basis Weight:

n/a



Caliper:

0.0034 inches ± 10%



Tensile:

MD 3,000 psi
CD 3,500 psi



Tear:

n/a



Stiffness:

n/a

Adhesive:
Fasson® S4600 is a clear general purpose permanent adhesive featuring good initial tack and ultimate adhesion to a wide variety of substrates. Meets the requirements of FDA 21 CFR 175.105 for indirect food contact.



Type:

Emulsion Acrylic



Minimum Application Temperature:

+10° F



Service Temperature Range:

-40° F to + 300° F subject to facestock limitations

Typical Performance Data: 2 Mil Clear Polyester at room temperature on standard lab panels


Stainless Steel
Loop Tack:
Peel Adhesion:


2.77 lbs
4.1 lbs


Aluminum
Loop Tack:
Peel Adhesion:


N/A
4.4 lbs


Alkyd Enamel Paint
Loop Tack:
Peel Adhesion:


N/A
3.9 lbs


Polypropylene
Loop Tack:
Peel Adhesion:


N/A
4.3 lbs


HDPE
Loop Tack:
Peel Adhesion:


N/A
4.6 lbs

Liner:
96#MF is a bleached, coated-two-side liner. Suitable for diecutting and stripping at moderate press speeds.



Basis Weight:

96# per ream ±10%
(500 sheets 25" x 38")



Caliper:

0.0070 inches ±10%



Tensile:

N/A



Tear:

MD 65 grams
CD 85 grams

Total Construction Caliper (approximate): 0.00113 inches ± 10%

Printing and Converting
To maximize on-press efficiencies when converting Fasson® laser film product constructions, material should be run with Grain Direction (machine direction) perpendicular to the Feed Direction of laser printing. For a comprehensive list of recommendations for laser products, see “Laser Product Converting Tips” at www.fasson.com. Please read this set of on-line converting tips before purchasing this product: http://na.fasson.com/frna/frnasite.nsf/PG/LNB1C5_NLaser_Guidelines?OpenDocument

Optimal Storage Conditions
Unless otherwise specified in this document, ideally store at 72F and 50% RH

Statement of Practical Use
All materials, sales and contracts for sale of Avery Dennison products are sold with the express requirement and understanding that the customer is solely and exclusively responsible for testing and for ensuring the products are fit for the customer's purposes or an end-user's purposes. All express or implied warranties of merchantability and fitness for particular use are disclaimed.

Warranty
All sales and contracts for sale are expressly conditioned on the buyer’s assent to Avery Dennison’s terms and conditions found on its website at label.averydennison.com/products. Avery Dennison hereby objects to any term, different from or additional to Avery Dennison’s terms, contained in any buyer communication in any form, unless agreed to in a writing signed by an officer of Avery Dennison.



label.averydennison.com

Label and Packaging Materials-North America
8080 Norton Parkway
Mentor, OH 44060
800-944-8511